  • Does 4010na/cb/Nr composite increase thermo-oxidative aging resistance?
  • The results shall indicate that, in comparison with 4010NA/CB/NR composite, there existed synergistic effect of antioxidant 4010NA and silica in 4010NA/SiO2 /NR composite on greatly enhancing thermo-oxidative aging resistance of NR material.
  • Which raw materials are used to prepare Nr & 4010na blends?
  • To avoid the disturbance of other additives, we only used raw materials NR, filler (CB or SiO 2 ), and antioxidant 4010NA to prepare NR, 4010NA/NR, CB/NR, 4010NA/CB/NR, SiO 2 /NR, and 4010NA/SiO 2 /NR blends. The weight loss of these blends were measured by TGA at 150 °C under nitrogen atmosphere.
  • What are the future trends of rubber antioxidants?
  • The perspectives on the future trends of rubber antioxidants have been presented. Elastomers, especially diene-rubbers containing unsaturated double carbon bonds in the main chains, are vulnerable to thermal/oxygen aging, which would make the elastomers less elastic and result in earlier failure of the elastomer products.
  • Can hydroxytoluene stop the autocatalytic aging reaction of rubber?
  • For instance, as shown in Fig. 1 b, butylated hydroxytoluene (BHT) could donate a hydrogen atom and convert peroxy radical to hydroperoxide, and therefore it could stop the autocatalytic aging reaction of rubber by blocking the propagation of peroxy radicals (Fig. 1 b), each BHT consumes two peroxy radicals. 3.